1.4980

1.4980

A 959 S66286, S66286, SUH 660, 1.4980, X6NiCrTiMoVB25.15.2, 1.2779,

1.4980数据表下载

1.4980化学成分 - EN 10302: 2008

C Cr Ni Mo Ti V B Mn Fe Al Si P S
≤0.08 13.50-16.00 24.00-27.00 1.00-1.50 1.75-2.30 0.10-0.50 0.001-0.010 1.00-2.00 ≤Bal ≤0.40 ≤1.00 ≤0.030 ≤0.020

1.4980标准规范

  • EN 10302: 2008 - Creep resisting steels, nickel and cobalt alloys
  • EN 10269: 1999 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • EN 10088-1: 2005 - Stainless steels. List of stainless steels

1.4980机械性能

热处理 最小值 最大值 近似值 备注
热处理 最小值 最大值 近似值 备注
热处理 最小值 最大值 近似值 备注
热处理 最小值 最大值 近似值 备注
热处理 最小值 最大值 近似值 备注
热处理 Type 最小值 最大值 近似值 备注
Note: a cold pull rods, round cakes and ring blank standard (Ti) 1.80% ~ 2.35%.
2 (B) of hot-rolled and cold-rolled sheet standard 0.003% ~ 0.010%, 2.00% or less (Mn), (P) acuities were 0.020%, 0.015% or less (S).
3 (Al) of cold drawn wire standard acuities were 0.35%, 1.75% ~ 2.35% (Ti) and (Si) 0.40% ~ 1.00%, 0.020% or less (P), (S) of 0.015% or less.
Use the wire, cold heading standards (Ti) 1.75% ~ 2.35%, 0.40% ~ 1.00% (Si), (P) acuities were 0.025%, 0.020% or less (S).
5 hot rolled and forged bar standard (Cu) of 0.25% or less.
1.5), heat treatment system is the standard heat treatment system are shown in table 1-3;Alloy is 900 ℃ heat treatment system plus or minus 10 ℃, 1 to 2 h, oil cooled to + 750 ℃ + 10 ℃, 16 h, air cooling.

1.4980库存信息

钢号 规格mm 重量kg
660B Ф90 1200
660B Ф95 1030
660B Ф100 1001
660B Ф110 2211
660B Ф130 3565
660B Ф140 1211
660B Φ90 260
660B Φ100 986
660B Ф44 698
660B Ф45 1588
660B Ф49 1685
660B Ф50 368
660B Ф60 2638
660B Ф80 1232
660B Ф85 1338
660B Ф25
660B Ф28 -
660B Ф35 -
660B Ф40 1132
660B Ф70 986
660B Ф75 1100
660B Ф80 850

1.4980产品形态